Uniform particle size, Nuclear grade mixed bed resin for water treatment in Nuclear power industry
SEPLITE® Monojet™ MB870NK Mixed Bed Resin Descriptions:
SEPLITE® Monojet™ MB870NK is a nuclear grade pre-mixed resin which is specifically designed for use in the highest purity water treatment in nuclear power industry, composed of capacity equivalent mixture of strongly acidic cation (SAC) and strongly basic (type I) gel anion (SBA) resins. The resins are highly regenerated and specially cleaned in order to comply with the specifications of producing high purified water, reduce the inorganic impurities to the lowest level as well as removing the traces of soluble organic compounds.
With its uniform particle size which enables excellent kinetic performance and high service flow rate, the low fines result in very low pressure losses compared with Gaussian distributed resins.
The resin applications include primary water treatment, fuel pool purification and PWR steam generation blowdown, BWR condensate polishing and Rad waste treatment.
SEPLITE® Monojet™ MB870NK Mixed Bed Resin Physical and Chemical Characteristics:
Components | Monojet™ SC7900N H | Monojet™ SA8800N OH |
Matrix Structure | Gel, Styrene-divinylbenzene | Gel, Styrene-divinylbenzene |
Functional group | Sulfonic acid | Quaternary amine |
Shipping form | H+ | OH- |
Physical Appearance | Amber to brownish translucent spherical beads | |
Particle size (mm) | 0.55±0.05mm | 0.63±0.05mm |
Moisture content (%) | 35-43 (H+ Form) | 54-60 (OH- Form) |
Total Capacity(eq/L) | ≥2.5 (H+ Form) | ≥1.2 (OH- Form) |
Ionic Conversion (%) | >99 | >95 |
Cation/Anion chemical equivalent ratio | 1:1 | |
Bulk density (g/L) | 700-750 | |
Whole beads count (%) | ≥95 | ≥95 |
Uniform coefficient | <1.2 | <1.2 |
Purity (Metals in dry basis) | Na ≤ 20 mg/kg | Na ≤ 20 mg/kg |
K ≤ 20 mg/kg | K ≤ 20 mg/kg | |
Fe ≤ 20 mg/kg | Fe ≤ 20 mg/kg | |
Cu ≤ 5 mg/kg | Cu ≤ 5 mg/kg | |
Co ≤ 5 mg/kg | Co ≤ 5 mg/kg | |
Ca ≤ 10 mg/kg | Ca ≤ 10 mg/kg | |
Mg ≤ 10 mg/kg | Mg ≤ 10 mg/kg | |
Al ≤ 10 mg/kg | Al ≤ 10 mg/kg | |
Hg ≤ 20 mg/kg | Hg ≤ 20 mg/kg | |
Heavy Metals (as Pb) ≤ 10 mg/kg | Heavy Metals (as Pb) ≤ 10 mg/kg | |
Cl ≤ 250 mg/kg | ||
SiO2 ≤ 10 mg/kg |
SEPLITE® Monojet™ MB870NK Mixed Bed Resin Precautions:
Resins should be stored in sealed containers or bags where temperature was above 0â?in dry conditions without exposure to direct sunlight. Do not mix ion exchange resin with strong oxidizing agents; otherwise it will cause violent reactions.
In case of eyes contact with resins, rinse eyes immediately with plenty of water, and consult a specialist. Material and samples must be disposed according to local regulations.
Dry polymers will expand when become wetted and may cause an exothermic reaction. Spilled materials may be slippery.
SEPLITE® and Monojet™ are registered trademarks of Sunresin New Materials Co. Ltd., Xi`an
-
This information is general information and may differ from that based on actual conditions. For more information about SEPLITE® resins, please contact SUNRESIN® directly.