SEPLITE® FN5504H
SEPLITE® FN5504H range covers mesh size of 50-100, 100-200, 200-400 strong acid cation resins, the cross-linkage is 4%.
This category resins are produced by the suspension polymerization technology same as standard resins just by selectively control. It provides excellent kinetic and packing properties, and maximum resistance to oxidation, reduction, mechanical wear and breakage.
The resins are produced fully in accordance with the FDA (US Food & Drug Administration), also meeting the regulations prescribed under Resolution ResAP (2004) 3 on ion exchange and adsorbent resins used in the processing of foodstuffs.
Please follow our start-up recommendations which is available upon request, when using our products in food applications.
SEPLITE® FN5504H Strong Acid Cation Resins Physical and Chemical Characteristics:
Product name | FN5504H(50-100) | FN5504H(100-200) | FN5504H(200-400) |
Matrix Structure | Polystyrene Crosslinked with DVB | Polystyrene Crosslinked with DVB | Polystyrene Crosslinked with DVB |
Functional group | Sulfonic acid | Sulfonic acid | Sulfonic acid |
Shipping form | H+ | H+ | H+ |
Physical Appearance | Yellow to claybank Spherical beads | Yellow to claybank Spherical beads | Yellow to claybank Spherical beads |
Mesh size | 50-100 | 100-200 | 200-400 |
Moisture content (%) | 60-70 | 60-70 | 60-70 |
Total Capacity(eq/L) | ≥1.1 | ≥1.1 | ≥1.1 |
Bulk Density ( g/l) (lbs/ft3) |
740 | 740 | 740 |
46 | 46 | 46 |
SEPLITE® FN5504H Strong Acid Cation Resins Package Options:
-
1 ft3 bag
-
50 liters blue drum
-
200 liters blue drum
SEPLITE® FN5504H Strong Acid Cation Resins Precautions:
Resins should be stored in sealed containers or bags where temperature was above 0℃ in dry conditions without exposure to direct sunlight. Do not mix ion exchange resin with strong oxidizing agents; otherwise it will cause violent reactions.
In case of eyes contact with resins, rinse eyes immediately with plenty of water, and consult a specialist. Material and samples must be disposed according to local regulations.
Dry polymers will expand when become wetted and may cause an exothermic reaction. Spilled materials may be slippery.
SEPLITE® and Monojet™ are registered trademarks of Sunresin New Materials Co. Ltd., Xi`an
-
This information is general information and may differ from that based on actual conditions. For more information about SEPLITE® resins, please contact SUNRESIN® directly.
All information set forth herein is for informational purposes only. This information is general descriptive(introductory) information of SUNRESIN and its related products, technologies and services. Neither shall constitute the guarantee of SUNRESIN and its affiliates to products, technologies and services in specific fields and specific application conditions results, unless otherwise expressly noted. SUNRESIN and its affiliates assumes no obligation or liability for the information in this document. Customer is responsible for judging whether the information is appropriate for Customer's concrete demand and are obliged to understand whether the use of these products, technologies and services is permitted by the laws and regulations of their countries and relevant regions. Unless expressly stated, no freedom from infringement of use any patent or trademark or intellectual property rights owned by SUNRESIN or its affiliated companies under this document is to be inferred.